| Nominālais lielums (collas) | SCH5S | SCH10S | SCH10 | SCH20 | Sch30 | SCH40S | Stdot | SCH40 | sch60 | SCH80S | XS | Sch80 | SCH100 | SCH120 | SCH140 | SCH160 | Xxs | SCH160S |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 1/8 | 10.29 | - | 1.24 | - | - | 1.73 | 1.73 | 1.73 | 2.41 | 2.41 | 2.41 | - | - | - | - | - | - | - |
| 1/4 | 13.72 | - | 1.65 | - | - | 2.24 | 2.24 | 2.24 | 3.02 | 3.02 | 3.02 | - | - | - | - | - | - | - |
| 3/8 | 17.15 | - | 1.65 | - | - | 2.31 | 2.31 | 2.31 | 3.20 | 3.20 | 3.20 | - | - | - | - | - | - | - |
| 1/2(15) | 21.34 | 1.65 | 2.11 | - | - | 2.77 | 2.77 | 2.77 | 3.73 | 3.73 | 3.73 | - | - | - | 4.78 | 7.47 | 4.78 | - |
| 3/4(20) | 26.67 | 1.65 | 2.11 | - | - | 2.87 | 2.87 | 2.87 | 3.91 | 3.91 | 3.91 | - | - | - | 5.56 | 7.82 | 5.56 | - |
| 1(25) | 33.40 | 1.65 | 2.77 | - | - | 3.38 | 3.38 | 3.38 | 4.55 | 4.55 | 4.55 | - | - | - | 6.35 | 9.09 | 6.35 | - |
| 1 1/4(32) | 42.16 | 1.65 | 2.77 | - | - | 3.56 | 3.56 | 3.56 | 4.85 | 4.85 | 4.85 | - | - | - | - | 9.70 | - | - |
| 1 1/2(40) | 48.26 | 1.65 | 2.77 | - | - | 3.68 | 3.68 | 3.68 | 5.08 | 5.08 | 5.08 | - | - | - | - | 7.14 | 15.15 | 7.14 |
| 2(50) | 60.33 | 1.65 | 2.77 | - | - | 3.91 | 3.91 | 3.91 | 5.54 | 5.54 | 5.54 | - | - | - | - | 9.14 | 11.07 | 8.74 |
| 2 1/2(65) | 73.03 | 2.11 | 3.05 | - | - | 5.16 | 5.16 | 5.16 | 7.01 | 7.01 | 7.01 | - | - | - | - | 9.53 | 14.02 | 9.53 |
| 3(80) | 88.90 | 2.11 | 3.05 | - | - | 5.74 | 5.74 | 5.74 | 7.62 | 7.62 | 7.62 | - | - | - | - | 11.13 | 15.24 | 11.13 |
| 3 1/2(90) | 101.60 | 2.11 | 3.05 | - | - | 6.02 | 6.02 | 6.02 | 8.56 | 8.56 | 8.56 | - | - | - | 11.12 | 13.49 | 17.12 | 13.49 |
| 4(100) | 114.30 | 2.11 | 3.05 | - | - | 6.02 | 6.02 | 6.02 | 8.56 | 8.56 | 8.56 | - | - | - | 11.12 | 13.49 | 17.12 | 13.49 |
| 5(125) | 141.30 | 2.77 | 3.40 | - | - | 6.55 | 6.55 | 6.55 | 9.53 | 9.53 | 9.53 | - | - | - | 12.70 | 15.88 | 19.05 | 15.88 |
| 6(150) | 168.27 | 2.77 | 3.40 | - | - | 7.11 | 7.11 | 7.11 | 10.97 | 10.97 | 10.97 | - | - | - | 14.09 | 19.27 | 18.62 | 19.27 |
| 8(200) | 219.08 | 2.77 | 3.76 | 6.35 | 7.04 | 8.18 | 8.18 | 9.18 | 13.20 | 12.70 | 12.70 | 15.09 | 19.26 | 20.62 | 23.81 | 22.23 | 23.81 | |
| 10(250) | 273.05 | 3.40 | 4.19 | 6.35 | 7.80 | 9.27 | 9.27 | 9.27 | 12.70 | 12.70 | 12.70 | 15.09 | 19.26 | 21.44 | 25.40 | 28.58 | 25.40 | |
| 12(300) | 323.85 | 3.96 | 4.67 | 6.35 | 8.38 | 9.53 | 9.53 | 10.31 | 14.27 | 12.70 | 12.70 | 17.48 | 21.44 | 25.40 | 28.58 | 33.32 | 25.40 | |
| 14(350) | 355.60 | 3.96 | 4.78 | 6.35 | 7.92 | 9.53 | 9.53 | 11.13 | 15.09 | 12.70 | 12.70 | 19.05 | 23.81 | 27.79 | 31.75 | 35.71 | 25.40 | |
| 16(400) | 406.40 | 4.19 | 4.78 | 6.35 | 7.92 | 9.53 | 9.53 | 12.70 | 16.66 | 12.70 | 12.70 | 21.44 | 28.39 | 30.96 | 35.53 | 40.49 | 25.40 | |
| 18(450) | 457.20 | 4.19 | 4.78 | 6.35 | 7.92 | 11.13 | 9.53 | 14.27 | 19.05 | 12.70 | 12.70 | 23.81 | 29.36 | 34.33 | 38.67 | 45.24 | 25.40 | |
| 20(500) | 508.00 | 4.78 | 5.54 | 6.35 | 9.53 | 12.70 | 9.53 | 15.09 | 20.62 | 12.70 | 12.70 | 26.19 | 32.54 | 38.10 | 44.45 | 50.01 | 25.40 | |
| 22(550) | 558.80 | 4.78 | 5.54 | 6.35 | 9.53 | 12.70 | 9.53 | 22.23 | 12.70 | 12.70 | 28.58 | 34.93 | 41.26 | 47.63 | 53.98 | 25.40 | - | |
| 24(600) | 609.60 | 5.54 | 6.35 | 6.35 | 9.53 | 14.27 | 9.53 | 17.48 | 24.61 | 12.70 | 12.70 | 30.96 | 38.89 | 46.02 | 52.37 | 59.54 | - | |
| 26(650) | 660.40 | - | - | 7.92 | 12.70 | - | 9.53 | - | - | 12.70 | 12.70 | - | - | - | - | - | - | - |
| 28(700) | 711.20 | - | - | 7.92 | 12.70 | - | 9.53 | - | - | 12.70 | 12.70 | - | - | - | - | - | - | - |
| 30(750) | 762.00 | - | - | 7.92 | 12.70 | - | 9.53 | - | - | 12.70 | 12.70 | - | - | - | - | - | - | - |
| 32(800) | 812.80 | 6.35 | 7.92 | 7.92 | 12.70 | - | 9.53 | 17.48 | 12.70 | 12.70 | - | - | - | - | - | - | - | - |
| 34(850) | 863.60 | - | - | 7.92 | 12.70 | - | 9.53 | 17.48 | 12.70 | 12.70 | - | - | - | - | - | - | - | - |
| 36(900) | 914.40 | - | - | 7.92 | 12.70 | - | 9.53 | 19.05 | 12.70 | 12.70 | - | - | - | - | - | - | - | - |
| 40(1000) | 1016.00 | - | - | 9.53 | 14.3 | - | 9.53 | 26.20 | - | - | - | - | - | - | - | - | - | - |
Kāda ir atšķirība starp nominālo un collu nerūsējošā tērauda caurulēm?
Nominālais izmērs (DN):
Parasti izteikts milimetros (mm), nominālais izmērs attiecas uz aptuveno diametru vai caurules diametru.
Tā ir nominālā vērtība, nevis caurules faktiskais lielums. Piemēram,DN50norāda, ka nominālais diametrs ir aptuveni 50 mm, bet faktiskais ārējais diametrs varētu būt60,3 mm, atkarībā no sienas biezuma.
Nominālie izmēri tiek plaši izmantoti starptautiskos standartos, īpaši Eiropā un Āzijā.
Collas lielums (NP):
Izsakot collas (collas), collas izmērs attiecas uz nominālo caurules izmēru (NP).
Šo nosaukšanas konvenciju parasti izmanto tādās imperatora sistēmas valstīs kā Amerikas Savienotās Valstis.
Piemēram,NPS 1caurulei ir faktiskais ārējais diametrs33,4 mm, nevis 1 collas (25,4 mm).
Nosūtīt pieprasījumu